Fuselage aft electrical channels enclosed
Workshop temperature 25 deg C and humidity 39 %.
50g resin and 19g hardner was mixed with glass bubbles to make a batch of micro-slurry.
Micro-slurry was applied to the bottom and sides of the foam pieces.
The foam was positioned in place and covered with wax paper and weights added during cure.