Workshop temperature was 25 deg C and humidity 50%. A batch of epoxy was made using 140g resin and 53g hardner. The 6-ply of UND cloth was wet out with the epoxy. Epoxy was applied to the bulkheads where the layups are positioned. Flox was mixed with the epoxy in a small cup then applied …